UNS N10675 Corrosion-Resisting Superalloy Bars and Plates

This high nickel-molybdenum austenitic corrosion-resistant alloy possesses outstanding resistance to strong reducing acids. With low impurity content and stable single-phase structure, it has superior hot & cold formability and weldability, good resistance to stress corrosion cracking in reducing media, ideal for pressure-bearing equipment under heavy reducing corrosion.

Applications of UNS N10675

Widely used in hydrochloric acid reactors, hydrometallurgical leaching tanks, complete pickling equipment, phosphoric acid concentration heat exchangers, hydrofluoric acid treatment units and strong-reducing corrosion reactors for organic synthesis, serving as a dedicated pressure-bearing alloy for service environments with high-concentration reducing acids.

Equivalent Grades and Commonly Used Specifications of UNS N10675

Steel Grade Specification Specification Name
NS3203 GB/T 15007 Designations of corrosion-resistant alloy
UNS N10675 ASTM B564 Standard Specification for Nickel Alloy Forgings
ASTM B472 Standard Specification for Nickel Alloy Billets and Bars for Reforging
ASTM B335 Standard Specification for Nickel-Molybdenum Alloy Rod
ASTM B333 Standard Specification for Nickel-Molybdenum Alloy Plate, Sheet, and Strip
ASTM B619 Standard Specification for Welded Nickel and Nickel-Cobalt Alloy Pipe
ASTM B622 Standard Specification for Seamless Nickel and Nickel-Cobalt Alloy Pipe and Tube
ASTM B366 Standard Specification for Factory-Made Wrought Nickel and Nickel Alloy Fittings
ASTM B462 Standard Specification for Forged or Rolled Nickel Alloy Pipe Flanges, Forged Fittings, and Valves and Parts for Corrosive Service
Products produced as per other specifications or technical agreements (if need) are available.

Typical Chemical Composition of UNS N10675

Elements

C Cr P S Si Ni Mn Mo Cu Co Fe Al V Ni+Mo Nb Ta Ti W

Zr

Mass Fraction%

≤0.010 1.00~3.00 ≤0.030 ≤0.010 ≤0.10 ≥65.00 ≤3.00 27.00~32.0 ≤0.20 ≤3.00 1.00~3.00 ≤0.50 ≤0.20 94.00~98.00 ≤0.20 ≤0.20 ≤0.20 ≤3.00

≤0.10

Products produced as per other specifications or technical agreements (if need) are available.

Typical Heat Treatment Condition and Mechanical Properties of UNS N10675

Delivery Condition

Mechanical Properties and Hardness of Heat-Treated Specimens
Rp0.2/(N/mm2) Rm/(N/mm2) A/% Zb/% Aku2d/J HBR

HRC

Solution Annealed Condition

≥350 ≥760 ≥40 / / /

/

 Products produced as per other specifications or technical agreements (if need) are available.

Product Forms and Size Range of UNS N10675

Product forms

Size range

Bars

Diameter or side length: 5.0mm~1000mm
Flats

thickness: 4.0mm~1000mm

width: 300mm~2200mm

Produce as other form and size according to technical requirements are available.